Thermal annealing of photoluminescent Si deposited on silica aerogels

Publication Type

Journal Article

Authors

Abstract

Photoluminescence (PL) of chemically vapor deposited Si on silica aerogels has been investigated as a function of annealing temperature up to 650°C in air. The PL peak red shifts considerably with temperatures up to 350°C and then slightly blue shifts above 350°C. There are at least two different oxidation stages in the thermal annealing of porous Si: surface oxidation below 350°C, which results in higher luminescence yield particularly for large Si particles, and internal oxidation above 350°C, which reduces the effective particle size.

Journal

Solid State Communications

Volume

91

Year of Publication

1994

Notes

0038-1098doi: DOI: 10.1016/0038-1098(94)90564-9